Item |
Test conditions | Test method | Test data | unit |
Density | ISO 1183:1987 | 1040 | kg/m3 | |
Water absorption | ISO 62:1999 | <0.1 | % | |
Melt flow rate | 200°C/5kg | ISO 1133:1997 | 3.8 | cm3/10min |
Process shrinkage | ISO 294-4:1997 | 0.4-0.6 | % | |
Charpy impact strength | 1eU | ISO 179:1993 | 15 | kj/m2 |
Tensile modulus | 1mm/min | ISO 527-2:1993 | 3300 | MPa |
Elongation | 50mm/min | ISO 527-2:1993 | 3 | % |
Tensile strength at break | 50mm/min | ISO 527-2:1993 | 55 | MPa |
Ball indentation hardness H | 358N/30s | ISO 2039-1:1993 | 150 | N/mm2 |
Bending strength | 2mm/min | ISO 178:1993 | 100 | MPa |
HDT | 1.8MPa | ISO 75-2:1993 | 84 | °C |
Linear coefficient of thermal expansion | (23-80)°C | DIN 53 752 | 0.8-1.0 | K-1 |
Heat conduction | DIN 52 612 | 0.16 | W/mK | |
Vicat softening point | B50/oil | ISO 306:1994 | 93 | °C |
Item |
Testing standards |
Test Conditions |
Units | PG-22 | PG-33 | PG-80 | PG-80N |
Melt flow index |
D-1238 | 200°C*5kg | g/10min. | 17.5 | 7.4 | 4.0 | 5.7 |
Softening point |
D-1525 | 1kg. | °C | 87.0 | 94.0 | 97.7 | 97.6 |
Tensile strength |
D-638 | Kg/cm² | 420 | 470 | 500 | 490 | |
Tensile modulus |
D-638 | - | 26460 | 26220 | 26720 | 26720 | |
Bending strength |
D-790 | - | Kg/cm² | 540 | 670 | 690 | 690 |
Flexural modulus |
D-790 | Kg/cm² | 31000 | 31000 | 31000 | 31000 | |
Heat distortion temperature |
D-648 | - | °C | 75 | 79 | 81 | 81 |